A Ceramic Pinch for Molybdenum
Got something to say to this podcast? Send a voicemail, and you might hear yourself on the next episode! Episode 93 of the Professor Alex Volinsky podcast. 2.5 wt% ZrTiO4 in molybdenum pins grain boundaries and deflects cracks: rolled strength past 1000 MPa, 25% elongation annealed, 166% more than the lightly dosed alloy; too much ceramic turns particles into crack starters. Based on the paper: ZrTiO4 secondary phase effects on ductility and toughness of molybdenum alloys; B. Hu, J. Han, S. Ge, X. Hua, S. Li, H. Xing, K. Wang, P. Hu, J. Fu, W. Zhang, A.A. Volinsky; Materials Letters, 2022, Vol. 307, 131077. Hosts Elena and Marcus. AI-generated voices.