Coating Away Voltage Decay
Got something to say to this podcast? Send a voicemail, and you might hear yourself on the next episode! Episode 161 of the Professor Alex Volinsky podcast. A ~5 nm LiAl5O8 coating on a Li-rich cathode suppressed voltage decay: 243.5 mAh/g, 82.63% first-cycle efficiency, 95.8% capacity after 100 cycles vs 82.8% uncoated — the layer blocks HF attack and oxygen loss. Full 8-author published list used, including Fang Yang and Shengzeng Lin, omitted from the corpus record. Based on the paper: Suppressed voltage decay and improved electrochemical performance by coating LiAl5O8 on the surface of Li1.2Mn0.54Ni0.13Co0.13O2; Fang Yang, Shengzeng Lin, Zhimeng Guo, Yanru Shao, Biao Zhang, Xiaodong Zhang, Shuhao Yan, Alex A. Volinsky; Journal of Alloys and Compounds, 2019, Vol. 805, pp. 1034–1043. Hosts Elena and Marcus. AI-generated voices.