Mapping Copper's Hot Window
Got something to say to this podcast? Send a voicemail, and you might hear yourself on the next episode! Episode 133 of the Professor Alex Volinsky podcast. Hot deformation maps the safe forging window for a Cu-1.0Co-0.65Si-0.1Ti alloy: cobalt-silicide precipitates strengthen, titanium refines grains, and processing maps separate clean recrystallization from cracking. Measured values pending abstract retrieval. Based on the paper: Microstructure Evolution of Cu-1.0Co-0.65Si-0.1Ti Alloy During Hot Deformation; Y. Geng, X. Li, Y. Zhang, Y. Jia, H. Zhou, B. Tian, Y. Liu, A.A. Volinsky, X. Zhang, K. Song, P. Liu, X. Chen; Vacuum, 2020, Vol. 177, article 109376. Hosts Elena and Marcus. AI-generated voices.